The Influence of [Mn/S] Ratios on the Fracture Morphology of a Heavy-section Steel Castings at Elevated Temperature

대형주강의 고온파단형태에 미치는 [Mn/S]비의 영향

Sung-gyoo Kim, Ji-Tae Kim*, Bong-gyu Park and Heung-il Park†

Department of Materials System Engineering, Pukyung National University,*Samyoung M-Tek Co., Ltd

DOI : http://dx.doi.org/10.7777/jkfs.2014.34.5.170

Abstract

Using the Gleeble test, the effects of [Mn/S] ratios and the presence of sulfides on the high-temperature fracture morphology of heavy-section steel castings were analysed via analysed via the observations of the microstructures. The specimens for which the [Mn/S] ratio was in the range of 60~80 showed a ductile fracture morphology with an area reduction reduction of more than 60%, while some specimens with similar [Mn/S] ratios showed a brittle fracture morphology with an area reduction of 0.0% due to the liquidation of sulfides at the grain boundary. The fracture morphology was classified into three types in the Gleeble high-temperature tensile test specimens. The first type showed dimple formation at the grain boundary, the formation of globular MnS sulfides, and plastic deformation of sulfides at an elevated temperature, indicating a needle-point type of ductile fracture with area reductions of 96.0~97.8%. The second type was a knife-edge edge type brittle fracture with an area reduction of 0.0% due to the film-type liquidation of sulfides at the grain boundary, band-type liquidation, and the liquidation of a terraced nipple pattern. The third type was the typical ductile fracture with an area reduction of 31.3~81.0%, in accordance with the mixture of dimples with in the g grains and terraced nipple pattern at the grain boundary.

Keywords

Steel castings, Fracture morphology, [Mn/S] Ratios, Gleeble test